Overcharge of the TSWB cell

The diagram shows the overcharge of the TSWB cell and the temperature increase.

The cell is overcharged (after already being fully charged) gradually to 5V, 6V and 8V per cell. The temperature is monitored. The temperature reaches some 130*C.

The total time of the test is 30 minutes. During the test the cell did not explode, did not start burning, did not set itself on fire.

The TSWB cells are the most safe and reliable LFP cells with 10-year history of 10000+ customers.

(0 votes)
This article was helpful
This article was not helpful

Comments (0)
Post a new comment
 
 
Full Name:
Email:
Comments:
CAPTCHA Verification 
 
Please enter the text you see in the image into the textbox below. This is required to prevent automated registrations and form submissions.

Help Desk Software by Kayako Case
ERROR: This domain name does not match domain registered in the license key file (apache5.gwl.eu), allowed domains: 127.0.0.1,192.168.5.36,support.i4wifi.cz,support.gwl.eu,kayako.gwl.eu, please change the product path to match the domain under Admin CP > Settings > General Settings
This product will not work properly unless untill that value is changed.

For more information please contact Kayako support at https://my.kayako.com